Ushbu blogda biz etkazib berish bilan tanishamizASME B16.9 standarti bo'yicha ishlab chiqarilgan 254SMO armatura. 254SMO, shuningdek, UNS S31254 yoki Alloy 254 nomi bilan ham tanilgan, oʻta ostenitik zanglamaydigan poʻlatdir, ogʻir sharoitlarda korroziyaga chidamliligi bilan mashhur. ASME B16.9 ning qat'iy spetsifikatsiyalari bilan birlashtirilgan ushbu armatura kimyoviy ishlov berish, neft va gaz va dengiz ilovalari uchun echimlarni taklif qiladi.

 

ASME B169 254SMO Fittings Supply

 

254SMO materialiga umumiy nuqtai

 

254SMO yuqori-qotishma ostenitik zanglamaydigan po'latdir, ayniqsa, xloridga boy va kislotali sharoitlarda chuqurchalar, yoriqlar korroziyasi va stressli korroziya yorilishiga yuqori qarshilik ko'rsatish uchun mo'ljallangan.

 

Uning kimyoviy tarkibi taxminan 19,5-20,5% xrom, 17,5-18,5% nikel, 6,0-6,5% molibden, 0,18-0,22% azot va 0,50-1,00% misni o'z ichiga oladi, bunda uglerod miqdori past (maksimal 0,02% karbid miqdorini kamaytiradi)

 

Overview of 254SMO Material

 

Mexanik jihatdan u 650-680 MPa minimal tortishish kuchi, 300 MPa oquvchanlik va 35% cho'zilish qobiliyatini namoyon qiladi, bu uni mustahkam va egiluvchan qiladi. Bu xususiyatlar uning molibden va azotning yaxshilanishi bilan bog'liq bo'lib, 42,5 dan katta yoki unga teng bo'lgan chuqurlikka qarshilik ekvivalent soniga (PREN) erishadi, 316L kabi standart ostenitik navlardan ancha yuqori.

 

ASME B16.9 bo'yicha armatura sifatida ishlab chiqarilganda, 254SMO bosim ko'rsatkichlari, bardoshlik va sinov talablariga muvofiqligini ta'minlaydi, bu uni yuqori yaxlit quvur tizimlari uchun ideal qiladi.

 

254SMO buttweld armatura turlari

 

Ishlab chiqaruvchilar quvur tizimlarida yo'nalishni o'zgartirish, filial ulanishlari va diametrli o'tishlarni osonlashtirish uchun 254SMO paypoqli armaturalarni etkazib beradi. Ular birinchi navbatda ASTM A403 / ASME SA403 bo'yicha ishlab chiqarilgan, ostenitik zanglamaydigan po'latdan yasalgan quvur armatura uchun standart spetsifikatsiya.

 

254SMO Buttweld Fittings Types

 

Tirsaklar:Oqim yo'nalishini o'zgartirish uchun ishlatiladi. Ular uzoq radius (LR) va qisqa radius (SR) variantlari bilan standart 90{4}} va 45{5}} graduslik burchaklarda mavjud. Uzun radiusli tirsaklar nominal quvur o'lchamidan 1,5 baravar kattaroq markazdan yuzma-yuz o'lchamga ega, qisqa radiusli tirsaklar esa quvur o'lchamiga teng radiusga ega. Maxsus oqim talablari uchun 3D, 5D va 180 graduslik qaytib burmalar kabi maxsus tirsaklar ham mavjud.

 

Tees:Ular filiallarga ulanish imkonini beradi. Teng Tees bir xil o'lchamdagi uchta rozetkaga ega, Reducing Tees esa asosiy ishga tushirishdan kichikroq filial rozetkasiga ega.

 

Reduktorlar:Quvur diametrini o'zgartirishga yordam bering. Konsentrik reduktorlar nosimmetrik bo'lib, umumiy markaz chizig'iga ega, eksantrik reduktorlar esa bir tekis tomonga ega bo'lib, quvur oqimining yuqori yoki pastki qismini ushlab turish uchun ishlatiladi.

 

Qopqoqlar:Ular quvurning uchini doimiy ravishda muhrlab qo'yadi.

 

Qopqoq uchlari (boʻgʻim uchlari):Tizimda murvatli ulanish nuqtasini yaratish uchun lap qo'shma gardishlar bilan ishlatiladi.

 

Xochlar:Bir nuqtada uchrashadigan to'rtta quvur uchun ulanishlarni ta'minlang.

 

254SMO armatura spetsifikatsiyasi va o'lchamlari

 

254SMO ASME B16.9 armaturalari uchun texnik xususiyatlar zarb qilingan ostenitik zanglamaydigan po'lat uchun ASTM A403 WP-S31254 ga mos keladi, devor qalinligi bosim talablariga qarab 10S dan 160 gacha yoki XXS jadvaliga mos keladi.

 

UMUMIY Izoh: Barcha o'lchamlar millimetrda.

 

To'g'ri tee o'lchamlari Va xochlar

 

Nominal quvur hajmi

(NPS)

DN

Tashqi diametri

Bevelda

Markazdan-oxirigacha-

Yugurish, C

Chiqish, M [Izohlar (1) va (2)]

1/2

15

21.3

25

25

3/4

20

26.7

29

29

1

25

33.4

38

38

1 1/4

32

42.2

48

48

1 1/2

40

48.3

57

57

2

50

60.3

64

64

2 1/2

65

73.0

76

76

3

80

88.9

86

86

3 1/2

90

101.6

95

95

4

100

114.3

105

105

5

125

141.3

124

124

6

150

168.3

143

143

8

200

219.1

178

178

10

250

273.0

216

216

12

300

323.8

254

254

14

350

355.6

279

279

16

400

406.4

305

305

18

450

457

343

343

20

500

508

381

381

22

550

559

419

419

24

600

610

432

432

26

650

660

495

495

28

700

711

521

521

30

750

762

559

559

32

800

813

597

597

34

850

864

635

635

36

900

914

673

673

38

950

965

711

711

40

1000

1016

749

749

42

1050

1067

762

711

44

1100

1118

813

762

46

1150

1168

851

800

48

1200

1219

889

838

 

Qisqa radiusli tirsaklarning o'lchamlari

 

Nominal quvur hajmi (NPS)

DN

Beveldagi tashqi diametri

Markazdan-oxirigacha-, A

1

25

33.4

25

1 1/4

32

42.2

32

1 1/2

40

48.3

38

2

50

60.3

51

2 1/2

65

73.0

64

3

80

88.9

76

3 1/2

90

101.6

89

4

100

114.3

102

5

125

141.3

127

6

150

168.3

152

8

200

219.1

203

10

250

273.0

254

12

300

323.8

305

14

350

355.6

356

16

400

406.4

406

18

450

457

457

20

500

508

508

22

550

559

559

24

600

610

610

 

Qisqa radiusning o'lchamlari 180 daraja qaytishns

 

Nominal

Quvur

Hajmi

(NPS)

DN

Tashqarida

Diametri

Bevelda

Markaz-

-ga

markaz,

O

Orqaga - -

Yuz,

K

1

25

33.4

51

41

1 1/4

32

42.2

64

52

1 1/2

40

48.3

76

62

2

50

60.3

102

81

2 1/2

65

73.0

127

100

3

80

88.9

152

121

3 1/2

90

101.6

178

140

4

100

114.3

203

159

5

125

141.3

254

197

6

150

168.3

305

237

8

200

219.1

406

313

10

250

273.0

508

391

12

300

323.8

610

467

14

350

355.6

711

533

16

400

406.4

813

610

18

450

457

914

686

20

500

508

1016

762

22

550

559

1118

838

24

600

610

1219

914

 

Chiqish teelarini kamaytirish va chiqish xochlarini kamaytirish o'lchamlari

 

Nominal Quvur Hajmi

(NPS)

DN

Tashqarida Diametri da Bevel

Yugurish Chiqish

Markazdan-oxirigacha-

Yugurish, C

Chiqish, M [Eslatma (1)]

1/2 x 1/2 x 3/8

15 × 15 × 10

21.3

17.3

25

25

1/2 x1/2 x 1/4

15 × 15 × 8

21.3

13.7

25

25

3/4 x 3/4 x1/2

20 × 20 × 15

26.7

21.3

29

29

3/4 x 3/4 x 3/8

20 × 20 × 10

26.7

17.3

29

29

1 × 1 x 3/4

25 × 25 × 20

33.4

26.7

38

38

1 × 1 x 1/2

25 × 25 × 15

33.4

21.3

38

38

1 1/4 x 1 1/4 × 1

32 × 32 × 25

42.2

33.4

48

48

1 1/4 × 1 1/4 × 3/4

32 × 32 × 20

42.2

26.7

48

48

1 1/4 x 1 1/4 x 1/2

32 × 32 × 15

42.2

21.3

48

48

1 1/2 x 1 1/2 x 1/4

40 × 40 × 32

48.3

42.2

57

57

1 1/2 x 1 1/2 × 1

40 × 40 × 25

48.3

33.4

57

57

1 1/2 x 1 1/2 x 3/4

40 × 40 × 20

48.3

26.7

57

57

1 1/2 x 1 1/2x 1/2

40 × 40 × 15

48.3

21.3

57

57

2 × 2 × 1 1/2

50 × 50 × 40

60.3

48.3

64

60

2 × 2 × 1 1/4

50 × 50 × 32

60.3

42.2

64

57

2 × 2 × 1

50 × 50 × 25

60.3

33.4

64

51

2 × 2 × 3/4

50 × 50 × 20

60.3

26.7

64

44

2 1/2 x 2 1/2 × 2

65 × 65 × 50

73.0

60.3

76

70

2 1/2 x 2 1/2 x 1 1/2

65 × 65 × 40

73.0

48.3

76

67

2 1/2 × 2 1/2 × 1 1/4

65 × 65 × 32

73.0

42.2

76

64

2 1/2 × 2 1/2 × 1

65 × 65 × 25

73.0

33.4

76

57

3 × 3 × 2 1/2

80 × 80 × 65

88.9

73.0

86

83

3 × 3 × 2

80 × 80 × 50

88.9

60.3

86

76

3 × 3 × 1 1/2

80 × 80 × 40

88.9

48.3

86

73

3 × 3 × 1 1/4

80 × 80 × 32

88.9

42.2

86

70

3 1/2 x 3 1/2 × 3

90 × 90 × 80

101.6

88.9

95

92

3 1/2 × 3 1/2 × 2 1/2

90 × 90 × 65

101.6

73.0

95

89

3 1/2 × 3 1/2 × 2

90 × 90 × 50

101.6

60.3

95

83

3 1/2 × 3 1/2 × 1 1/2

90 × 90 × 40

101.6

48.3

95

79

4 × 4 × 3 1/2

100 × 100 × 90

114.3

101.6

105

102

4 × 4 × 3

100 × 100 × 80

114.3

88.9

105

98

4 × 4 × 2 1/2

100 × 100 × 65

113.3

73.0

105

95

4 × 4 × 2

100 × 100 × 50

114.3

60.3

105

89

4 × 4 × 1 1/2

100 × 100 × 40

114.3

48.3

105

86

5 × 5 × 4

125 × 125 × 100

141.3

114.3

125

117

5 × 5 × 3 1/2

125 × 125 × 90

141.3

101.6

124

114

5 × 5 × 3

125 × 125 × 80

141.3

88.9

124

111

5 × 5 × 2 1/2

125 × 125 × 65

141.3

73.0

124

108

5 × 5 × 2

125 × 125 × 50

141.3

60.3

124

105

 

Reduktorlarning o'lchamlari

 

Nominal quvur

Hajmi (NPS)

DN

Tashqarida

Diametri da

Bevel

Oxirigacha--oxirigacha,

H

Nominal quvur

Hajmi (NPS)

DN

Tashqarida

Diametri da

Bevel

Oxirigacha--oxirigacha,

H

Katta

Oxiri

Kichik

Oxiri

Katta

Oxiri

Kichik

Oxiri

3/4 x 1/2

20 ×15

26.7

21.3

38

5 × 4

125 ×100

141.3

114.3

127

3/4 x 3/8

20 ×10

26.7

17.3

38

5 × 3 1/2

125 ×90

141.3

101.6

127

1 × 3/4

25 ×20

33.4

26.7

51

5 × 3

125 ×80

141.3

88.9

127

1 × 1/2

25 ×15

33.4

21.3

51

5 × 2 1/2

125 ×65

141.3

73.0

127

1 1/4 × 1

32 ×25

42.2

33.4

51

5 × 2

125 × 50

141.3

60.3

127

1 1/4 ×3/4

32 ×20

42.2

26.7

51

6 × 5

150 ×125

168.3

141.3

140

1 1/4 x 1/2

32 ×15

42.2

21.3

51

6 × 4

150 ×100

168.3

114.3

140

1 1/2 x 1 1/4

40 ×32

48.3

42.2

64

6 × 3 1/2

150 ×90

168.3

101.6

140

1 1/2 × 1

40 ×25

48.3

33.4

64

6 × 3

150 ×80

168.3

88.9

140

1 1/2 x 3/4

40 ×20

48.3

26.7

64

6 × 2 1/2

150 ×65

168.3

73.0

140

1 1/2 x 1/2

40 ×15

48.3

21.3

64

8 × 6

200 ×150

219.1

168.3

152

2 ×1 1/2

50 ×40

60.3

48.3

76

8 × 5

200 ×125

219.1

141.3

152

2 ×1 1/4

50 ×32

60.3

42.2

76

8 × 4

200 ×100

219.1

114.3

152

2 × 1

50 ×25

60.3

33.4

76

8 × 3 1/2

200 ×90

219.1

101.6

152

2 ×3/4

50 ×20

60.3

26.7

76

10 × 8

250 ×200

273.0

219.1

178

2 1/2 x 2

65 ×50

73.0

60.3

89

10 × 6

250 ×150

273.0

168.3

178

2 1/2 x 1 1/2

65 ×40

73.0

48.3

89

10 × 5

250 x 125

273.0

141.3

178

2 1/2 x 1 1/4

65 ×32

73.0

42.2

89

10 × 4

250 ×100

273.0

114.3

178

2 1/2 × 1

65 ×25

73.0

33.4

89

12 × 10

300 ×250

323.8

273.0

203

3 ×2 1/2

80 ×65

88.9

73.0

89

12 × 8

300 ×200

323.8

219.1

203

3 × 2

80 ×50

88.9

60.3

89

12 × 6

300 ×150

323.8

168.3

203

3 × 1 1/2

80 ×40

88.9

48.3

89

12 × 5

300 ×125

323.8

141.3

203

3 × 1 1/4

80 ×32

88.9

42.2

89

14 × 12

350 ×300

355.6

323.8

330

3 1/2 × 3

90 ×80

101.6

88.9

102

14 × 10

350 ×250

355.6

273.0

330

3 1/2 x 2 1/2

90 ×65

101.6

73.0

102

14 × 8

350 ×200

355.6

219.1

330

3 1/2 × 2

90 ×50

101.6

60.3

102

14 × 6

350 ×150

355.6

168.3

330

3 1/2 × 1 1/2

90 ×40

101.6

48.3

102

16 × 14

400 ×350

406.4

355.6

356

3 1/2 x 2 1/4

90 ×32

101.6

42.2

102

16 × 12

400 ×300

406.4

323.8

356

4 × 3 1/2

100 ×90

114.3

101.6

102

16 × 10

400 ×250

406.4

273.0

356

4 × 3

100 ×80

114.3

88.9

102

16 × 8

400 ×200

406.4

219.1

356

4 × 2 1/2

100 ×65

114.3

73.0

102

18 × 16

450 ×400

457

406.4

381

4 × 2

100 ×50

114.3

60.3

102

18 × 14

450 ×350

457

355.6

381

4 ×1 1/2

100 ×40

114.3

48.3

102

18 × 12

18 × 10

450 ×300

450 ×250

457

457

323.8

273.0

381

381

 

Uzun radiusning oʻlchamlari-Tirsaklarni qisqartirish

 

Nominal

Quvur

Hajmi

(NPS)

DN

Tashqi diametri

Bevelda

Markaz-

-Oxiriga,

A

Nominal

Quvur

Hajmi

(NPS)

DN

Tashqi diametri

Bevelda

Markaz-

-Oxiriga,

A

Katta oxiri

Kichik oxiri

Katta oxiri

Kichik oxiri

2 × 1 1/2

50 × 40

60.3

48.3

76

10 × 8

250 × 200

273.0

219.1

381

2 × 1 1/4

50 × 32

60.3

42.2

76

10 × 6

250 × 150

273.0

168.3

381

2 × 1

50 × 25

60.3

33.4

76

10 × 5

250 × 125

273.0

141.3

381

2 1/2 × 2

65 × 50

73.0

60.3

95

12 × 10

300 × 250

323.8

273.0

457

2 1/2 × 1 1/2

65 × 40

73.0

48.3

95

12 × 8

300 × 200

323.8

219.1

457

2 1/2 × 1 1/4

65 × 32

73.0

42.2

95

12 × 6

300 × 150

323.8

168.3

457

3 × 2 1/2

80 × 65

88.9

73.0

114

14 × 12

350 × 300

355.6

323.8

533

3 × 2

80 × 50

88.9

60.3

114

14 × 10

350 × 250

355.6

273.0

533

3 × 1 1/2

80 × 40

88.9

48.3

114

14 × 8

350 × 200

355.6

219.1

533

3 1/2 × 3

90 × 80

101.6

88.9

133

16 × 14

400 × 350

406.4

355.6

610

3 1/2 × 2 1/2

90 × 65

101.6

73.0

133

16 × 12

400 × 300

406.4

323.8

610

3 1/2 × 2

90 × 50

101.6

60.3

133

16 × 10

400 × 250

406.4

273.0

610

4 × 3 1/2

100 × 90

114.3

101.6

152

18 × 16

450 × 400

457

406.4

686

4 × 3

100 × 80

114.3

88.9

152

18 × 14

450 × 350

457

355.6

686

4 × 2 1/2

100 × 65

114.3

73.0

152

18 × 12

450 × 300

457

323.8

686

4 × 2

100 × 50

114.3

60.3

152

18 × 10

450 × 250

457

273.0

686

5 × 4

125 × 100

141.3

114.3

190

20 × 18

500 × 450

508

457

762

5 × 3 1/2

125 × 90

141.3

101.6

190

20 × 16

500 × 400

508

406.4

762

5 × 3

125 × 80

141.3

88.9

190

20 × 14

500 × 350

508

355.6

762

5 × 2 1/2

125 × 65

141.3

73.0

190

20 × 12

500 × 300

508

323.8

762

6 × 5

150 × 125

168.3

141.3

229

20 × 10

500 × 250

610

273.0

762

6 × 4

150 × 100

168.3

114.3

229

24 × 22

600 × 550

610

559

914

6 × 3 1/2

150 × 90

168.3

101.6

229

24 × 20

600 × 500

610

508

914

6 × 3

150 × 80

168.3

88.9

229

24 × 18

600 × 450

610

457

914

8 × 6

200 × 150

219.1

168.3

305

24 × 16

600 × 400

610

406.4

914

8 × 5

200 × 125

219.1

141.3

305

24 × 14

600 × 350

610

355.6

914

8 × 4

200 × 100

219.1

114.3

305

24 × 12

600 × 300

610

323.8

914

 

Uzun radiusli tirsakning o'lchamlari

 

Nominal quvur hajmi (NPS)

DN

Tashqarida

Diametri

Bevelda

Markazdan-oxirigacha-

90 daraja

Tirsaklar, A

45 daraja

Tirsaklar, B

1/2

15

21.3

38

16

3/4

20

26.7

38

19

1

25

33.4

38

22

1 1/4

32

42.2

48

25

1 1/2

40

48.3

57

29

2

50

60.3

76

35

2 1/2

65

73.0

95

44

3

80

88.9

114

51

3 1/2

90

101.6

133

57

4

100

114.3

152

64

5

125

141.3

190

79

6

150

168.3

229

95

8

200

219.1

305

127

10

250

273.0

381

159

12

300

323.8

457

190

14

350

355.6

533

222

16

400

406.4

610

254

18

450

457

686

286

20

500

508

762

318

22

550

559

838

343

24

600

610

914

381

26

650

660

991

405

28

700

711

1067

438

30

750

762

1143

470

32

800

813

1219

502

34

850

864

1295

533

36

900

914

1372

565

38

950

965

1448

600

40

1000

1016

1524

632

42

1050

1067

1600

660

44

1100

1118

1676

695

46

1150

1168

1753

727

48

1200

1219

1829

759

 

Lap qo'shma tayoq uchlarining o'lchamlari

 

Nominal Quvur Hajmi(NPS)

DN

Tashqarida Diametri ning Barrel

Uzoq Naqsh Uzunlik, F[Eslatmalar (3),

(4)]

Qisqa Naqsh Uzunlik, F[Eslatmalar (3),

(4)]

Radius ning Fileto, R[Eslatma

(5)]

Diametri ning Lap, G[Eslatma

(6)]

Maks.

Min.

1/2

15

22.8

20.5

76

51

3

35

3/4

20

28.1

25.9

76

51

3

43

1

25

35.0

32.6

102

51

3

51

1 1/4

32

43.6

41.4

102

51

5

64

1 1/2

40

49.9

47.5

102

51

6

73

2

50

62.4

59.5

152

64

8

92

2 1/2

65

75.3

72.2

152

64

8

106

3

80

91.3

88.1

152

64

10

127

3 1/2

90

104.0

100.8

152

76

10

140

4

100

116.7

113.5

152

76

11

157

5

125

144.3

140.5

203

76

11

185

6

150

171.3

167.5

203

89

13

218

8

200

222.1

218.3

203

102

13

270

10

250

277.2

272.3

254

127

13

324

12

300

328.0

323.1

254

152

13

381

14

350

359.9

354.8

305

152

13

413

16

400

411.0

405.6

305

152

13

470

18

450

462

456

305

152

13

533

20

500

514

507

305

152

13

584

22

550

565

558

305

152

13

641

24

600

616

609

305

152

13

692

 

Qopqoqlarning o'lchamlari

 

Nominal

Quvur hajmi

(NPS)

 

DN

Tashqarida

Diametri

Bevelda

Uzunlik, E

[Izoh (1)]

Cheklovchi devor

Qalinligi uchun

Uzunlik, E

Uzunlik, E

[Izoh (2)]

1/2

3/4 1

1 1/4

1 1/2

2

2 1/2

3

3 1/2

4

5

6

8

10

12

14

16

18

20

22

24

26

28

30

32

34

36

38

40

42

44

46

48

15

20

25

32

40

50

65

80

90

100

125

150

200

250

300

350

400

450

500

550

600

650

700

750

800

850

900

950

1000

1050

1100

1150

1200

21.3

26.7

33.4

42.2

48.3

60.3

73.0

88.9

101.6

114.3

141.3

168.3

219.1

273.0

323.8

355.6

406.4

457

508

559

610

660

711

762

813

864

914

965

1016

1067

1118

1168

1219

25

25

38

38

38

38

38

51

64

64

76

89

102

127

152

165

178

203

229

254

267

267

267

267

267

267

267

305

305

305

343

343

343

4.57

3.81

4.57

4.83

5.08

5.59

7.11

7.62

8.13

8.64

9.65

10.92

12.70

12.70

12.70

12.70

12.70

12.70

12.70

12.70

12.70

. . .

. . .

. . .

. . .

 

. . .

. . .

. . .

. . .

. . .

 

. . .

. . .

. . .

25

25

38

38

38

44

51

64

76

76

89

102

127

152

178

191

203

229

254

254

305

. . .

. . .

. . .

. . .

 

. . .

. . .

. . .

. . .

. . .

 

. . .

. . .

. . .

 

Xulosa

 

Umid qilamanki, ushbu batafsil qo'llanma sizning xaridlaringiz va muhandislik ehtiyojlaringiz uchun foydalidir. Batafsil spetsifikatsiya tafsilotlari uchun 254SMO armaturalarining turli jadvallari uchun bosim{1}}harorat ko‘rsatkichlarining batafsil taqsimoti bilan qiziqasizmi?

 

So'rov yuborish
Bizga keling
Va endi RFQSni boshlang.
Biz bilan bog'lanish